MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Corning 7056 Alkali Borosilicate Crushed/Powdered Glass
Categories: Ceramic; Glass; Optical; Oxide; Silicon Oxide

Material Notes: Crushed/Powdered glass available in mesh sizes 4 through 325 and can be customized. Used primarily as a Kovar Sealing Glass. This product is used in MOEMS applications.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.29 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 62.8 GPa
Poissons Ratio 0.21
Shear Modulus 26.5 GPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.50e+8 ohm-cm
@Temperature 350 °C
 2.00e+10 ohm-cm
@Temperature 250 °C
Dielectric Constant 5.7
@Frequency 1e+6 Hz
Dissipation Factor 0.0027
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.15 µm/m-°C
@Temperature 0.000 - 300 °C
 5.45 µm/m-°C
@Temperature 25.0 - 679 °C
Set Point
Softening Point 718 °C107.6 Poise
Working Point 1058 °C104 Poise
Annealing Point 512 °C1013 Poise
Strain Point 472 °C1014 Poise
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.487
@Wavelength 589.3 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corning 7052 Alkali Barium Borosilicate Sealing Glass Powder
Borosilicate Glass, Low Expansion
Corning 7059 Barium Borosilicate Glass
Borosilicate Glass
Accuratus MACOR Machinable Glass Ceramic

CCORNG04 / 736

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.