MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec MZ 111 Zirconia, ZrO2-Y2O3
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications.

Key Words: Zirconium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.08 g/ccDIN EN 623-2
Water Absorption 0.00 %Open Porosity; DIN EN 623-2
Particle Size 0.15 - 0.20 µmGrain; DIN EN 623-3
Permeability 0.00%, Gas
Weibull Modulus >= 10DINV ENV 843-5
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 1250HV1; DINV ENV 843-4
 1250HV 0.5; DIN ENV 843-2
Tensile Modulus 210 GPaYoung's; DINV ENV 843-2
Flexural Strength 1050 MPaDIN EN 843-1
 1400 MPaBending Strength; 4-Point; without HIP: 1050; DIN ENV 843-1
Compressive Strength 2200 MPaDIN 51067T1
Poissons Ratio 0.30DINV ENV 843-2
Fracture Toughness 6.70 MPa-m½KIC (SEVNB); DIN CEN/TS 14425-1
 7.50 MPa-m½SEVNB; ISO 23 146
Shear Modulus 80.8 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 672-1
Dielectric Constant 29
@Frequency 1e+6 Hz
IEC 672-1
Dielectric Strength 19.0 kV/mmIEC 672-1
Dielectric Loss Index 0.0020
@Frequency 1e+9 Hz
IEC 672-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.1 µm/m-°C
@Temperature 20.0 - 100 °C
DIN EN 821-1
 11.2 µm/m-°C
@Temperature 20.0 - 400 °C
DIN EN 821-1
 11.6 µm/m-°C
@Temperature 20.0 - 600 °C
DIN EN 821-1
 11.7 µm/m-°C
@Temperature 20.0 - 1000 °C
DIN EN 821-1
Specific Heat Capacity 0.400 J/g-°CDINV ENV 821-3
Thermal Conductivity 2.50 W/m-KDIN EN 821-2
Maximum Service Temperature, Air 1000 °C
Maximum Service Temperature, Inert 1000 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 0.10 %DIN ISO 12677
HfO2 2.0 %DIN ISO 12677
Y2O3 4.9 %DIN ISO 12677
ZrO2 93 %DIN ISO 12677
 
Descriptive Properties
ColorIvory
Monoclinic Content (%)< 1DIN ISO 12677
Other Oxides (%)< 0.1DIN ISO 12677
Ra = Arithmetic Mean Roughness Value (µm)<0.06
Radioactivity (Bq/kg)10.2ISO 13 356
Thermal Shock Resistance R1 (K)336calculated; R1 = [σs (1-µ)] / (α·E)
Thermal Stress R2 (W/m)841

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec MZ 111 HIP Zirconia, ZrO2-Y2O3
MarkeTech Zirconium Oxide Ceramic - Zirconia, Y2O3 Stabilized
Yttria Stabilized Zirconia, YSZ
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
CeramTec MZ 429 Zirconia, ZrO2-Y2O3

CCERA910 / 107510

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.