MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics Tecksof 2000 Conductive Fabric Over Foam Gasket
Categories: Polymer

Material Notes: Description: The Tecknit TECKSOF 2000 Series gasket consists of conductive fabric over foam and has been designed to meet today’s commercial EMI shielding applications demands where wide tolerance gaps exist. The foam core is flexible and conformable, making it ideal for applications requiring low closure force and minimal compression set. Tecknit TECKSOF 2000 Series gaskets are ideal suited for commercial electronic enclosures.

Application Information: Conduct soft gaskets are an ideal low cost solution for placement in enclosures where weight and space are limited. TECKSOF 2000 is an excellent choice where conformability as well as high shielding requirements are specified. Applications recommended include electronic cabinets/enclosures, laptop computers, cellular devices and portable electronic devices such as PDA’s

Corrosion Resistance: Galvanic Compatiblity With Aluminum, Galvanized Steel, Electrogalvanized Steel and Other Materials

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity >= 5.0 cPASTM D2196
 
Mechanical PropertiesOriginal ValueComments
Compression Set >= 10 %Profile Dependent
 8.0 - 20 %
 30 - 40 %Typical
 <= 80 %Profile Dependent
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 0.050 ohmTypically
 <= 0.070 ohm
Shielding Effectiveness >= 100 dB
@Frequency 2.0e+7 - 1.00e+10 Hz
.25" x .375" Profiles; MIL-G-83528B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
Minimum Service Temperature, Air -40.0 °C
Brittleness Temperature -55.0 °CASTM D2137
Flammability, UL94 V-1Depending on Profile
 V-0Depending on Profile
 
Descriptive Properties
Extractable Silicone0.04

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
P & P Technology M W Conductive Fabric
P & P Technology MW Series Conductive Fabric
P & P Technology NF32B050A21 Nylon/PET/Cu+Ni Conductive Fabric
Parker Chomerics SOFT-SHIELD® 3700 High Temperature Conductive Fabric Over Foam
Abatron AboWeld 8708-8 One-Component Structural/Dielectric Epoxy

PCHOME422 / 131132

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.