MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Primex Plastics Prime PETG 14471 Polyethylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: Prime PETG 14471 is an economical high-clarity PETG co-polyester resin developed for thick sheet applications. The benefits of this material are excellent clarity, outstanding toughness, chemical resistance, cold formable without stress whitening, machinable, excellent thermoforming characteristics and it can be sealed with adhesives.

Applications: Include point of purchase, displays, store fixtures, indoor and outdoor signs, vending machine parts, and industrial, building, construction, and architectural components.

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 104104ASTM D785
Tensile Strength, Yield 53.1 MPa7700 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Flexural Modulus 2.14 GPa310 ksiASTM D790
Izod Impact, Notched  0.374 J/cm
@Temperature -30.0 °C
0.700 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 0.908 J/cm
@Temperature 22.8 °C
1.70 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C40.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 69.4 °C157 °FASTM D648
Vicat Softening Point 82.8 °C181 °FASTM D1525
Flammability, UL94  HB
@Thickness >=0.254 mm
HB
@Thickness >=0.0100 in
 V-2
@Thickness >=3.00 mm
V-2
@Thickness >=0.118 in
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRIM015 / 278486

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.