MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PCTFE Fluoro plastic
Categories: Polymer; Thermoplastic; Fluoropolymer; Polychlorotrifluoroethylene (PCTFE); Molded

Material Notes: General description: PCTFE (polychlorotrifluoroethylene) is a semi-crystalline polymer. As a rigid material, it appears to have a slightly yellowish/whitish translucency or is transparent depending on the fabrication process used. In comparison with PTFE, PCTFE is significantly harder and more dimensionally stable. It is the hardest of the fluoroplastics. Even at very low temperatures of around –255 °C, it retains its excellent dimensional stability. It also has the lowest gas permeability rate. PCTFE can be processed using injection moulding, extrusion presses, and thermoplastic extrusion.

Characteristics and properties:

  • Very wide temperature range - including very low temperatures - of –255 to +150 °C (brief exposure to +200 °C)
  • Very good mechanical strength; in particular, low creeping under compressive stress
  • Non-flammable, even at high oxygen concentrations (100% oxygen index limit)
  • High chemical resistance to mineral acid and a number of organic acids
  • Excellent resistance to ageing
  • Practically no moisture absorption and therefore very dimensionally stable
  • Impermeable to water and steam

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.14 g/ccDIN EN ISO 1183-1
Water Absorption at Saturation <= 0.050 %DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 34.0 - 50.0 MPaDIN EN ISO 527
Elongation at Break 120 - 175 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 1.40 GPaDIN EN ISO 527
Izod Impact, Unnotched 80.0 J/mASTM D 256-81
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmDIN IEC 60023
Surface Resistance 1.00e+16 ohmDIN IEC 60023
Dielectric Constant 2.5 - 2.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mmIEC 60243-1
Dielectric Loss Index 0.0090 - 0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 - 80.0 µm/m-°C
@Temperature 23.0 - 95.0 °C
DIN 53752
Melting Point 215 °C
Minimum Service Temperature, Air -250 °C
 
Descriptive Properties
Colornatural (white)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP093 / 250591

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.