MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color Only

Application: LCD Back Light Unit parts

CAS: 103598-77-2, 9003-56-9 and 13463-67-1

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccASTM D792
Maximum Moisture Content 0.020Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117ASTM D785
Tensile Strength, Yield 590 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 120 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 950 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Flexural Modulus 25000 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Izod Impact, Notched >= 65.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 0.00 - 60 secASTM D495
Comparative Tracking Index 400 - 600 V
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
 30 - 60 sec
@Thickness >=3.00 mm
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
 >= 120 arcs
@Thickness 3.00 mm
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 127 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 80.0 °C
@Thickness >=0.850 mm
 110 °C
@Thickness >=1.50 mm
 110 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 80.0 °C
@Thickness >=0.850 mm
 100 °C
@Thickness >=1.50 mm
 100 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 80.0 °C
@Thickness >=0.850 mm
 120 °C
@Thickness >=1.50 mm
 120 °C
@Thickness >=3.00 mm
Flammability, UL94 V-1
@Thickness >=0.850 mm
 V-0
@Thickness >=1.50 mm
 V-0
@Thickness >=3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 280 °CInjection Molding
Middle Barrel Temperature 260 - 290 °CInjection Molding
Front Barrel Temperature 260 - 290 °CInjection Molding
Nozzle Temperature 260 - 280 °CInjection Molding
Melt Temperature 260 - 280 °CInjection Molding
Mold Temperature 60.0 - 90.0 °CInjection Molding
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Back Pressure 0.981 - 3.92 MPaInjection Molding
Screw Speed 40 - 70 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance
Lotte Advanced Materials Infino® HN-1064IA PC, Unreinforced FR
Westlake Plastics Radel® R 5500 Polyphenylsulfone
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized

PLAY561 / 148571

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.