MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CMT Materials HYTAC® W Low Thermal Conductivity Epoxy Syntactic
Categories: Polymer; Thermoset; Epoxy

Material Notes: The use of syntactic materials as plug assist tooling replacing conventional materials such as aluminum, wood, felt or Delrin has become increasingly popular in the thermoforming industry. Syntactics, the combination of hollow glass spheres in a polymer matrix, have many unique properties that make them ideal candidates for both roll-fed and sheet-fed applications.

Low Thermal Conductivity and Specific Heat: This translates to lower heat transfer reducing warm-up time and virtually eliminating material sticking to the plug.

Dimensionally Stable: The low coefficient of thermal expansion means the plug maintains its shape over a wide temperature range.

Excellent Temperature Resistance: HYTAC-W is specially formulated with an epoxy resin which maintains a high modulus at elevated temperatures.

Lightweight: This increases the life of capital equipment due to reduced wear and tear on moving parts.

Easily Machined: HYTAC-W can be easily machined to any size or shape using conventional equipment.

Variety of Shapes and Sizes:The material is provided in standard sized rots or sheets, but may be custom molded to meet the specific needs.

Applications: HYTAC-W is often used for short run or price sensitive applications, providing cost effective, low thermal conductivity plugs for quick start up times, better material distribution, improved surface appearance and longer life than basic alternatives.

Recommended for use with PE, PS and PVC.

Information Provided by CMT Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 41.0 - 45.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Flexural Toughness 2.70 psiASTM D790
Compressive Strength 6200 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µin/in-°F
Thermal Conductivity 0.110 W/m-K
Maximum Service Temperature, Air 350 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Delrin® 588P NC010 Acetal (POM)
Tra-Con Tra-Bond K6 Ablative Thermal Epoxy Compound
Overview of materials for Epoxy, Molded, Mineral Filled
Molybdenum Carbide, Mo2C
Master Bond MB350 Alkoxyethyl Cyanoacrylate

PCMT001 / 93137

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.