MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CoorsTek Pure SiC™ HR CVD Silicon Carbide, > 99.9995%
Categories: Ceramic; Carbide

Material Notes: Data Provided by the manufacturer, CoorsTek, Inc.

Key Words: SiC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.21 g/ccASTM C20
Water Absorption 0.00 %ASTM 373
Particle Size 3.0 - 10 µmThin Section Crystal Size
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 271000 g
Modulus of Elasticity 462 GPaASTM C848
Flexural Strength 468 MPaASTM F417
Poissons Ratio 0.21ASTM C848
Fracture Toughness 3.50 MPa-m½Notched Beam
Shear Modulus 191 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+6 ohm-cmASTM D1829
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.60 µm/m-°C
@Temperature 25.0 - 1000 °C
ASTM C372
Specific Heat Capacity 0.665 J/g-°CASTM E1269
Thermal Conductivity 115 W/m-KASTM C408
Maximum Service Temperature, Air 1600 °CNo Load
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoorsTek Pure SiC™ LR CVD Silicon Carbide, > 99.9995%
Silicon Carbide, Alpha SiC
Silicon Carbide, CVD
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide

CZ3C2e / 2750

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.