MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Plating Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.03 - 2.50 g/ccAverage value: 1.09 g/cc Grade Count:35
Water Absorption 0.200 - 1.00 %Average value: 0.420 % Grade Count:5
Linear Mold Shrinkage 0.00300 - 0.00800 cm/cmAverage value: 0.00541 cm/cm Grade Count:29
Linear Mold Shrinkage, Transverse 0.00300 - 0.00800 cm/cmAverage value: 0.00587 cm/cm Grade Count:8
Melt Flow 1.20 - 45.0 g/10 minAverage value: 13.7 g/10 min Grade Count:34
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 101 - 116Average value: 108 Grade Count:22
Ball Indentation Hardness 74.0 - 100 MPaAverage value: 91.3 MPa Grade Count:6
Tensile Strength, Ultimate 20.0 - 48.0 MPaAverage value: 38.5 MPa Grade Count:21
Tensile Strength, Yield 36.0 - 63.0 MPaAverage value: 44.7 MPa Grade Count:27
Elongation at Break 3.00 - 70.0 %Average value: 26.0 % Grade Count:27
Elongation at Yield 2.00 - 7.00 %Average value: 4.08 % Grade Count:9
Modulus of Elasticity 1.70 - 2.77 GPaAverage value: 2.28 GPa Grade Count:16
Flexural Yield Strength 56.0 - 82.0 MPaAverage value: 68.1 MPa Grade Count:30
Flexural Modulus 1.96 - 5.47 GPaAverage value: 2.37 GPa Grade Count:36
Izod Impact, Notched 0.230 - 5.82 J/cmAverage value: 2.63 J/cm Grade Count:25
 0.5339 - 3.50 J/cm
@Temperature -40.0 - 0.000 °C
Average value: 1.08 J/cm Grade Count:2
 0.784532 - 0.980 J/cm
@Temperature -30.0 - -30.0 °C
Average value: 1.08 J/cm Grade Count:3
 0.784532 - 0.980 J/cm
@Thickness 3.17 - 12.7 mm
Average value: 1.08 J/cm Grade Count:3
Izod Impact, Unnotched 1.471 - 1.56906 J/cm
@Temperature -30.0 - -30.0 °C
Average value: 1.52 J/cm Grade Count:1
 1.471 - 1.56906 J/cm
@Thickness 3.20 - 6.40 mm
Average value: 1.52 J/cm Grade Count:1
Izod Impact, Notched (ISO) 16.4 - 58.0 kJ/m²Average value: 25.8 kJ/m² Grade Count:10
 7.00 - 41.0 kJ/m²
@Temperature -30.0 - -20.0 °C
Average value: 13.9 kJ/m² Grade Count:7
Charpy Impact Unnotched 17.0 J/cm² - NBAverage value: 17.0 J/cm² Grade Count:3
 11.0 - 15.0 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 13.0 J/cm² Grade Count:2
Charpy Impact, Notched 1.70 - 5.30 J/cm²Average value: 2.45 J/cm² Grade Count:13
 0.700 - 4.00 J/cm²
@Temperature -30.0 - -20.0 °C
Average value: 1.50 J/cm² Grade Count:7
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 - 1.00e+16 ohm-cmAverage value: 5.35e+15 ohm-cm Grade Count:6
Surface Resistance 1.00e+14 - 1.00e+16 ohmAverage value: 5.27e+15 ohm Grade Count:4
Dielectric Constant 2.90 - 3.00Average value: 2.96 Grade Count:3
Dielectric Strength 28.0 - 38.0 kV/mmAverage value: 33.3 kV/mm Grade Count:4
Dissipation Factor 0.00500 - 0.0150Average value: 0.00860 Grade Count:3
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 67.0 - 100 µm/m-°CAverage value: 85.6 µm/m-°C Grade Count:11
Thermal Conductivity 0.250 - 0.250 W/m-K
@Temperature 30.0 - 260 °C
Average value: 0.250 W/m-K Grade Count:1
Deflection Temperature at 0.46 MPa (66 psi) 87.8 - 113 °CAverage value: 96.5 °C Grade Count:16
Deflection Temperature at 1.8 MPa (264 psi) 76.1 - 203 °CAverage value: 92.6 °C Grade Count:35
Vicat Softening Point 90.0 - 115 °CAverage value: 101 °C Grade Count:28
UL RTI, Electrical 60.0 - 80.0 °CAverage value: 64.0 °C Grade Count:3
UL RTI, Mechanical with Impact 60.0 - 80.0 °CAverage value: 64.0 °C Grade Count:3
UL RTI, Mechanical without Impact 60.0 - 80.0 °CAverage value: 64.0 °C Grade Count:3
Flammability, UL94 HBGrade Count:28
Glow Wire Test 650 - 700 °CAverage value: 667 °C Grade Count:3
 
Optical PropertiesOriginal ValueComments
Gloss 90.0 - 98.0 %Average value: 95.5 % Grade Count:4
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 210 - 274 °CAverage value: 228 °C Grade Count:4
Melt Temperature 188 - 274 °CAverage value: 221 °C Grade Count:18
Mold Temperature 40.0 - 85.0 °CAverage value: 63.0 °C Grade Count:19
Injection Velocity 240 mm/secAverage value: 240 mm/sec Grade Count:4
Drying Temperature 70.0 - 93.3 °CAverage value: 84.0 °C Grade Count:16
Injection Pressure 4.83 - 150 MPaAverage value: 65.8 MPa Grade Count:10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

O1107 / 77798

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.