MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Hydex™ 202 Rigid Polyurethane (PU)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Hydex™ 202 is a totally rigid polyurethane resin that exhibits a broad range of chemical resistance, as well as superior impact and excellent mechanical properties. It can be used for any mechanical application that requires a combination of toughness, dimensional stability and chemical resistance. It has an ability to withstand chemical attack in a PH range from 2 to 14.

Information Provided by Ensinger, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.21 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8000 psiASTM D638
Tensile Strength, Yield 9000 psiASTM D638
Elongation at Break 80 %ASTM D638
Elongation at Yield 9.0 %ASTM D638
Tensile Modulus 240000 psiASTM D638
Flexural Strength 12000 psiASTM D790
Flexural Modulus 280000 psiASTM D790
Izod Impact, Notched 10.0 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.22SS counter surface
Coefficient of Friction, Static 0.26SS counter surface
 
Thermal PropertiesOriginal ValueComments
CTE, linear 37.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 290 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 280 °FASTM D648
Vicat Softening Point 292 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Hydex™ 301 Rigid Polyurethane (PU)
Covestro Baybond® PU 406 Polyurethane
Westlake Plastics Zelux® GS Polycarbonate - Gamma Stabilized For Medical Applications
YOUJU New Materials Paryls® PPSU F1150
YOUJU New Materials Paryls® PPSU F1350 High Flow

PENSIN059 / 104750

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.