INSPIRE TF7000 ES Natural Performance Polymer DA™ is a very high stiffness (2400 MPa) TPO designed for instrument panel upper and lower components, as well as other interior trim applications where stiffness, good impact resistance, and good molded-in-color part aesthetics are important. Its high melt flow rate also allows for rapid filling of large parts in the injection molding process. Main Characteristics: - Excellent Surface Aesthetics
- Good Scratch & Mar Resistance
- Instrument Panel Uppers/Lowers
- Interior Trim Applications
- High Flow
- Approved on DaimlerChrylser MS-DC265D
Automotive Specifications:- CHRYSLER MS-DC-265 Type D
- IMDS ID 30867190 Color: Charcoal
- GM QK 004023 U Color: Charcoal
Information provided by Trinseo. |