MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Styrofoam™ SM Extruded Polystyrene Foam Insulation
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: STYROFOAM™ Brand SM Extruded Polystyrene Foam Insulation is a multi-purpose extruded polystyrene board that helps to meet the needs of the commercial and residential foundation and slab market. The closed-cell structure of STYROFOAM™ Brand SM Insulation resists water absorption, enabling it to retain a high R-value (RSI) over time – a necessaryproperty in below-grade residential foundation applications.

STYROFOAM™ Brand SM Insulation helps to protect foundation dampproofing and waterproofing, especially during backfilling. It also provides a secondary barrier against groundwater leakage. With STYROFOAM™ Brand SM Insulation, the freeze-thaw cycling of the foundation wall is minimized, reducing the possibility of cracking. And a warmer foundation wall reduces the potential for condensation and adds to the thermal mass of the building.

This material is produced as sheets of closed-cell foam by a continuous extrusion process. Its properties will be different than expanded polystyrene beads because beads have voids between cell walls.

This former Dow product line is now a DuPont product line.

Key Words: Foundation and Underslab
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption >= 0.30 %volume%; ASTM C272
 <= 0.70 %volume%; ASTM D2842
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 30.0 psiASTM D1621
 
Thermal PropertiesOriginal ValueComments
CTE, linear 63.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Insulation R Value >= 7.5
@Thickness 38.1 mm
Standard Size (Imperial)
 >= 10
@Thickness 50.8 mm
Standard Size (Imperial)
 >= 12
@Thickness 61.0 mm
Standard Size (Imperial)
 >= 12.5
@Thickness 63.5 mm
Standard Size (Imperial)
 >= 15
@Thickness 76.2 mm
Standard Size (Imperial)
 >= 20
@Thickness 102 mm
Standard Size (Imperial)
 >= 5.0
@Thickness 25.4 mm,
Temperature 23.9 °C
Standard Size (Imperial); ASTM C518
Maximum Service Temperature, Air 74.0 °C
 
Descriptive Properties
Water Vapor Permeance90 ng/Pa-s-m² MaxASTM E96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Styrofoam™ Polystyrene Rigid Foam Insulation
DuPont Styrofoam™ Scoreboard Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Ultra SL Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Tongue and Groove Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Square Edge Extruded Polystyrene Foam Insulation

PDWZ00e / 209614

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.