MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 5115/SAE 5115 Low Alloy Steel, Case Hardened
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 5000 Series Steel

Key Words: UNS G51150. Comparable to ISO 683-11(87) 16MnCr5; Belgium NBN-253-03 16MnCr5; DIN 1652(90) 16MnCr5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 780 - 1080 MPa
@Thickness 30.0 mm
Case Hardened
 880 - 1230 MPa
@Thickness 16.0 mm
Case Hardened
Tensile Strength, Yield 590 MPa
@Thickness 30.0 mm
Case Hardened
 600 MPa
@Thickness 16.0 mm
Case Hardened
Elongation at Break 10 %
@Thickness 30.0 mm
Case Hardened
Modulus of Elasticity 200 GPaTypical of Alloy Steel
Poissons Ratio 0.29Typical of Alloy Steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°CTypical of Alloy Steel
Specific Heat Capacity 0.470 J/g-°CTypical of Alloy Steel
Thermal Conductivity 52.0 W/m-KTypical of Alloy Steel
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.10 %
Carbon, C 0.13 - 0.19 %
Chromium, Cr 0.80 - 1.1 %
Cobalt, Co <= 0.10 %
Copper, Cu <= 0.30 %
Iron, Fe 96.5 - 97.9 %As Balance
Manganese, Mn 1.0 - 1.3 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.40 %
Sulfur, S <= 0.035 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
16MnCr5 Alloy Steel
AISI 5115/SAE 5115 Low Alloy Steel, Cold Drawn Bar
AISI 1045 Steel, cold drawn, high temperature stress relieved, 50-75 mm (2-3 in) round
AISI 5117 Steel Composition Spec (UNS G51170)
Overview of materials for AISI 4000 Series Steel

M5115a / 231092

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.