MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis HE1344 High Density Polyethylene Compound for Cellular Insulation of Data Cables  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: HE1344 is a high-molecular weight, high-density polyethylene insulation compound containing an industry approved non plate-out chemical blowing agent. It contains the required levels and types of primary antioxidant and metal deactivator to satisfy most wire and cable standards for product longevity. HE1344 is capable of 50 percent density reduction.

Borcell1344 is designed for the production of foam or foam-skin insulation in either air-core or grease-filled copper cable constructions.

Former trade name for this product was Borcell™.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.480 g/ccExpanded Compound; ASTM D792
 0.945 g/ccCompound; ASTM D792
Oxidative Induction Time (OIT) 50 minAt 200°C, Al-pan; ASTM D3895
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1900 psiExpanded Compound; ASTM D638
 3300 psiCompound; ASTM D638
Elongation at Break 500 %Expanded Compound; ASTM D638
 600 %Compound; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.33
@Frequency 1e+6 Hz
ASTM D1531
Dissipation Factor 0.000040
@Frequency 1e+6 Hz
ASTM D1531

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis LE1120 Low Density Polyethylene for Physically Foamed Cellular Insulation
Borealis HE1345 High Density Polyethylene Compound for Cellular Insulation of Telephone Singles
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation
Borealis HE4873 High Density Polyethylene
Borealis Visico™/Ambicat™ LE4423/LE4476 Fast Curing, Easy Processing, Environmentally Friendly, Silane Crosslinkable LDPE Compound for Low Voltage Insulation

PBOREA028 / 27335

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.