MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay RHODAFAC® RE-610 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Extremely versatile. Moderate foaming. Good electrolyte tolerance, coupling properties and hard surface detergency. Useful in heavy-duty liquid cleaners of all types, dry cleaning, pesticide emulsions, and as dedusting agents for powdered detergents. Promote formation of PVAc and acrylics with film clarity, corrosion inhibition as well as light, heat and pH stability. Rhodafac PE-9 and Rhodafac R9-47A are industrial grades.

Chemical Name: PLOYXYETHYLENE NONYLPHENYL ETHER, BRANCHED PHOSPATE

CAS: 68412-53-3

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODAFAC RE-610 can be used to prepare a broad range of commercial emulsion polymers including acrylics, vinyl-acrylics and styrene-acrylics. Such polymers find application in latex paints, adhesives, paper coatings and textiles. RHODAFAC RE-610 is typically converted to its salt form (sodium, ammonium, amine) for use in emulsion polymerization. This is usually done in-situ by neutralization of the diluted phosphate ester with the desired base. Films of polymers make with RHODAFAC RE-610 exhibit enhanced corrosion resistance and superior heat and light stability, which makes them especially desirable for metal coating applications. The versatility of RHODAFAC RE-610 allows it to be used with a wide range of polymerization techniques, including thermal and redox processes. When properly used in conjunction with other anionic and nonionic surfactants, RHODAFAC RE-610 allows for the trouble-free commercial production of extremely stable emulsion polymers.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Surface Tension 37 dynes/cmat CMC
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 67 - 72KOH to First INFL. PT.; RP-0427
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.70 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear to slightly hazy liquidRP-0064
Color<200APHA, RP-0134
CompositionNonionic content<5%, RP-0351
Critical Micelle Concentration (%)0.01
Ionic ChargeAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODAFAC® RS-610 Surfactant
Solvay RHODAFAC® PA32 Surfactant
Solvay RHODAFAC® RE-610 E Surfactant
Solvay RHODAFAC® RS-710 E Surfactant
Solvay RHODAFAC® RS-710 Surfactant

WRHOD364 / 137595

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.