MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik ROHACELL® 71 SL Polymethacrylimide Foam
Categories: Polymer; Thermoset; Polymethacrylimide

Material Notes: The trend towards lighter, better performing and more robust equipment for many sports remains unbroken. Yet the manufacturing process to create these innovative new products must continue to be cost efficient and reliable. In many cases, these demanding requirements call for fibre-reinforced plastic (FRP) sandwich construction to deliver the ideal solution. Whether the goal is excellent bending stiffness and strength, stabilization of very thin FRP sheets against external forces, or generating complex 3-dimensional geometries with minimized effort - a ROHACELL® sandwich can do the trick.

Strength and durability: ROHACELL® SL boasts outstanding mechanical strength, especially under tensile load, and a high tenacity. These attributes make it a great choice for applications with substantial dynamic mechanical loads, as often found in sports and leisure equipment.

ROHACELL® helps you to save weight: The fine cell size minimizes the surface resin absorption while maintaining a strong connection to the face sheet. At the same time, the 100% closed cell structure keeps the resin where you want it – in the interface.

Fast and efficient processing: Excellent temperature stability facilitates processing at up to 180°C with all common processes like vacuum infusion and resin transfer molding, pre-preg autoclaving as well as hand lay-up. High curing temperatures allow for reduced cycle times and excellent laminate properties. ROHACELL® SL is easy to shape by routing and thermoforming.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0750 g/ccISO 845
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 4.20 MPaISO 527-2
Elongation at Break 6.1 %ISO 527-2
Tensile Modulus 134 MPaISO 527-2
Compressive Strain at Break 3.4 %ISO 844
Compressive Strength 1.30 MPaISO 844
Compressive Modulus 52.0 MPaISO 844
Shear Modulus 0.0330 GPaASTM C273
Shear Strength 1.50 MPa7.8% shear strain; ASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.5 µm/m-°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Rohacell® 71 IG-F Industrial Grade Polymethacrylimide (PMI) Foam
Evonik Rohacell® 71 HF High Frequency Grade Polymethacrylimide (PMI) Foam
Avient Edgetek® AS-20GF/000 HI UV NAT Acrylonitrile Butadiene Styrene (ABS), Glass Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
RTP Company RTP 600 Acrylonitrile Butadiene Styrene (ABS), Unfilled

PEVONIL317 / 196521

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.