MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® eXten D 437P PA6.10, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced material. This material is available in natural.

Benefits: This polyamide 6,10 for extrusion is specially performing where high flexibility and toughness are requested. It is specially developed for automotive and other applications where a long term high temperature usage is requested.

Key Properties: Translucency; UV stabilized; High impact at low temperature and High flexibility

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC This grade complies with RoHS directive 2002/95/EC Unless specified, this grade is not suitable for food contact, medical devices or toy applications

Applications: Extrusion pipes and tubing applications.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccISO 1183/A
Water Absorption 0.65 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Water Absorption at Saturation 1.9 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaISO 527 Type 1A
Tensile Strength, Yield 35.0 MPaISO 527 Type 1A
Elongation at Break >= 200 %ISO 527 Type 1A
Tensile Modulus 630 MPaISO 527 Type 1A
Flexural Modulus 470 MPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
Melting Point 215 °CISO 11357
 
Processing PropertiesOriginal ValueComments
Front Barrel Temperature 215 - 235 °C
Die Temperature 210 - 230 °C
Moisture Content <= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® B 230 PA66/6, Conditioned
Domo TECHNYL® eXten D 458P PA6.10, Conditioned
Domo TECHNYL® eXten D 437P PA6.10, Dry
Domo TECHNYL® B 238 Black 21 N PA66/6, Conditioned
Domo TECHNYL® B 50 H1 PA66/6, Conditioned

PRHOD557 / 137788

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.