MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Abatron AboWeld 8708-8 One-Component Structural/Dielectric Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Unreinforced; Epoxy, Thermally Conductive

Material Notes: AboWeld 8708-8 is a highly filled, class H (180°C) structural, heat-conductive adhesive paste for FAST high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; Embedding applications where 2-component systems are not practical; Appliances; Radiators; Electronic components; Medical equipment; Excellent bond to metals, ceramics, glass; Assembly; Patching; Filling; Resurfacing; Insulation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 15.0 lb/gal
Viscosity 1500 cP
@Temperature 100 °C
 180000 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 70
@Temperature 120 °C
 90
@Temperature 25.0 °C
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 400 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
Thermal Conductivity 5.28 BTU-in/hr-ft²-°F
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 min
@Temperature 180 °C
 40.0 min
@Temperature 150 °C
 120 - 180 min
@Temperature 121 °C
Shelf Life <= 5.00 Month
 
Descriptive Properties
ColorBlack
Hardening Time (min)12150°C
 4180°C
 60121°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron AboWeld 8708-5 One-Component Structural/Dielectric Epoxy
P & P Technology M W Conductive Fabric
Abatron AboWeld 8708-7 One-Component Structural/Dielectric Epoxy
Abatron AboCast 10-5/AboCure 50-12 Epoxy
Abatron AboCast 10-5/AboCure 3-4 Epoxy

PABC811 / 107795

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.