MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carlson 70 30 Cu Ni Copper-Nickel Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Nickel Alloy

Material Notes: General Description

Carlson alloy 70 30 Cu Ni is a copper nickel alloy with excellent resistance to corrosion and erosion. It is strong and ductile. 70 30 Cu Ni is utilized in areas where high temperatures and pressures, combined with high velocities and turbulence are serious problems. It can be utilized up to 700°F for ASME code heat exchangers and unfired pressure vessels.

70 30 Cu Ni exhibits outstanding resistance to general and impingent attack by clean sea water. It is, however, subject to bio-fouling at low velocities. 70 30 Cu Ni also has excellent resistance to attack by fresh water, boiler feedwater, and steam. It withstands the attack of phosphoric, sulfuric, and mild organic acids. It is attacked by chromic, hydrobromic, hydrochloric, and nitric acids. 70 30 Cu Ni is resistant to alkaline chlorides, chromates, nitrates and sulfates. It is, however, attacked by the cyanides and acid dichromates. 70 30 Cu Ni resists wet and dry chlorine, bromine, and carbon dioxide at ambient temperatures.

Applications

70 30 Cu Ni is widely used in marine service, tidewater power plants, desalinization plants, oil refineries, and in the chemical process industry. It is utilized extensively as a condenser and salt water tube and piping material for the U.S. Navy.

Product applications include condenser, heat exchanger and distiller tubes, tube sheets and baffles, sale water piping, water boxes, tanks, vats, pressure vessels, process equipment, pumps and valves.

Information provided by Carlson

Key Words: UNS C71500
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  310 MPa
@Thickness >=63.5 mm
45000 psi
@Thickness >=2.50 in
 >= 345 MPa
@Thickness <=63.5 mm
>= 50000 psi
@Thickness <=2.50 in
Tensile Strength, Yield  124 MPa
@Strain 0.2 %,
Thickness >=63.5 mm
18000 psi
@Strain 0.2 %,
Thickness >=2.50 in
 >= 138 MPa
@Strain 0.2 %,
Thickness <=63.5 mm
>= 20000 psi
@Strain 0.2 %,
Thickness <=2.50 in
Elongation at Break >= 35 %>= 35 %
Modulus of Elasticity 152 GPa22000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.050 %<= 0.050 %
Copper, Cu 64.39 - 70.6 %64.39 - 70.6 %
Iron, Fe 0.40 - 1.0 %0.40 - 1.0 %
Lead, Pb <= 0.020 %<= 0.020 %
Manganese, Mn <= 1.0 %<= 1.0 %
Nickel, Ni 29 - 33 %29 - 33 %
Phosphorus, P <= 0.020 %<= 0.020 %
Sulfur, S <= 0.020 %<= 0.020 %
Zinc, Zn <= 0.50 %<= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper nickel 30%, UNS C71500
Carlson 90 10 Cu Ni Copper-Nickel Alloy
Special Metals MONEL® 404 Copper-Nickel Alloy
304 Stainless Steel
Copper nickel 10%, UNS C70600

NCARLSO26 / 15833

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.