MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
AMG Aluminum BoralĀ® 8% Boron Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: With the use of master alloys containing special addition agents, many characteristics can be imparted to aluminum alloys. Master alloys containing beryllium are added to aluminum magnesium melts at low levels to reduce magnesium losses. Small beryllium additions also improve surface quality of DC billet as well as impart improved mechanical properties to premium quality aluminum casting. The electrical and thermal conductivity of aluminum can be improved by the addition of trace amounts of boron to eliminate the undesirable effects of chromium, titanium, vanadium and zirconium. Boron also provides an effective grain refiner for aluminum silicon alloys. The use of Aluminum Strontium to modify the silicon phase of hypoeutectic aluminum silicon casting alloys from coarse platelets to a fine fibrous structure is a widely accepted practice. This results in improved casting soundness and mechanical properties, particularly ductility.

Information provided by KB Alloys

Al. Assoc. Registration No: H2222

Former KB Alloys product. AMG acquired KB Alloys in 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 88.77 - 90.27 %
Boron, B 7.5 - 9.0 %
Iron, Fe 0.30 %
Other, each 0.030 %
Other, total 0.10 %
Potassium, K 1.0 %
Silicon, Si 0.25 %
Sodium, Na 0.50 %
Titanium, Ti >= 0.050 %
 
Descriptive Properties
FormWaffle Ingot

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NKBAL20 / 17690

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.