MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel
Categories: Metal; Ferrous Metal; Tool Steel; Hot Work Steel

Material Notes: Description: THERMODUR 2344 is a single melt Extra Fine Structure (EFS) hot work die steel; and Supplied in the annealed condition

Characteristics: Good toughness; Good resistance to thermal shock and fatigue; Good hardenability; and Good high-temperature strength

Applications: Hot forging dies, Hot extrusion tooling, Forming dies, Plastic molds and Shot sleeve

Stress Relieving (Heat Treatment): 1200°F for 2 hours; Cooling: Cool slowly to 930°F in air; Hardness: <230 HB

Hardening (Heat Treatment): 1850°F- 1880°F Hold at temperature for 30 minutes; Cooling: Vacuum quench to 1000°F then cool to below 150°F; Hardness: <54 HRC Quenched

Information provided by Schmolz + Bickenbach

Key Words: AISI H-13
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.281 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 34
@Treatment Temp. 700.0 °C,
Time 7200 sec
 42
@Treatment Temp. 650.0 °C,
Time 7200 sec
 50
@Treatment Temp. 600.0 °C,
Time 7200 sec
 54
@Treatment Temp. 400 °C,
Time 7200 sec
 54
@Treatment Temp. 550.0 °C,
Time 7200 sec
 56
@Treatment Temp. 500 °C,
Time 7200 sec
Tensile Strength 192 ksi42 HRC
 242 ksi50 HRC
 259 ksi52 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 µin/in-°F
@Temperature 21.1 - 93.3 °C
 6.60 µin/in-°F
@Temperature 21.1 - 204 °C
 7.00 µin/in-°F
@Temperature 21.1 - 399 °C
Thermal Conductivity 177 BTU-in/hr-ft²-°F
@Temperature 21.1 °C
 191 BTU-in/hr-ft²-°F
@Temperature 343 °C
 210 BTU-in/hr-ft²-°F
@Temperature 704 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 1380 - 1470 °FSoft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 230 HB
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 %
Chromium, Cr 5.3 %
Iron, Fe 90.9 %
Molybdenum, Mo 1.4 %
Silicon, Si 1.0 %
Vanadium, V 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel
Schmolz + Bickenbach Thermodur® 2344 Magnum Hot Work Die Steel
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel
Assab Steels DIEVAR Hot Work Steel
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel

NSCHMO012 / 125885

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.