MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: EVATANE 42-60 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE 42-60 is stabilized with antioxidants and contains slip and antiblock additives. EVATANE 42-60 is readily dissolved into solvent and can be used in inks or solvent adhesives. The High Vinyl Acetate content of EVATANE 42-60 brings softness, flexibility, polarity and high solubility.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/cc
@Temperature 23.0 °C
ISO 1183
Vinyl Acetate Content 41 - 44 %FTIR (internal)
Melt Index of Compound 55 - 80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 42ASTM D2240
Tensile Strength at Break 5.00 MPaASTM D638
Elongation at Break 900 - 1100 %ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 48.0 °CDSC
Vicat Softening Point <= 40.0 °C
@Load 1.02 kg
ISO 306
Ring & Ball Softening Point 95.0 °CASTM E28
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 230 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema EVATANE® 40-55 Copolymer Ethylene - Vinyl Acetate
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Dow Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin
Arkema Evatane® 1003 VL 2 Ethylene Vinyl Acetate
Arkema OREVAC® 9304 EVA Terpolymer

PARKG100 / 80145

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.