MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow Nd2Fe14B Neodymium Iron Boron Magnetic Material
Categories: Metal; Electronic/Magnetic Alloy; Intermetallic

Material Notes: Introduced in 1983, Neodymium-Iron-Boron magnet materials have become the material of choice for a wide range of permanent magnet devices and applications. The high Iron content makes them susceptible to corrosion, and they may need to be coated for some applications.

Information provided by Goodfellow

Key Words: Nd2Fe14B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 580kgf/mm²
Tensile Strength 75.0 MPa
Modulus of Elasticity 150 GPa
 
Electrical PropertiesOriginal ValueComments
Magnetic Coercive Force, Hc 875 - 1990 Oe
Magnetic Remanence, Br 1.0 - 1.3 Gauss
Curie Temperature 310 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.20 µm/m-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 9.00 W/m-K
@Temperature 23.0 °C
 
Component Elements PropertiesOriginal ValueComments
Boron, B 5.9 %Molar
Iron, Fe 82 %Molar
Neodymium, Nd 11.8 %Molar

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alliance N-33 Neodymium Iron Boron Magnetic Material
Alnico® 4 (Isotropic, Cast) Hard Magnetic Alloy
Cobalt Samarium 1 Hard Magnetic Alloy
Goodfellow Aluminum EN AC 42100
Molybdenum Disilicide, MoSi2

NGOODF178x / 197415

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.