MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum Moly Permalloy Electrical Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Nickel Alloy

Material Notes: An alloy with exceptionally high magnetic permeability, very low coercive force, very low core losses, and low reminance by magnetic field annealing. The alloy finds application in magnetic shielding where fields much less than the Earth's magnetic filed are required. The highest volume applications using laminations or tape wound cores today are ground fault interrupter and modem transformer cores. The alloy is used as well in a variety of other high performance transformer core applications such as tape recorder heads and audio transformers. Control of the cooling rate during heat treatment and superimposition of various customer bake treatments are used to develop the most suitable magnetic quality for the application.

Information provided by Allegheny Ludlum

Key Words: ASTM A-753; MIL-N-14411
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.25 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 80Typical Annealed
Tensile Strength, Ultimate 682 MPaTypical Annealed
Tensile Strength, Yield 338 MPa
@Strain 0.2 %
Typical; Annealed
Elongation at Break 32 %typical in 2"; Annealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000470 ohm-cm
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.010 %
Carbon, C 0.015 %
Chromium, Cr <= 0.020 %
Cobalt, Co <= 0.020 %
Iron, Fe 14 %as balance
Manganese, Mn 0.50 %
Molybdenum, Mo 4.85 %
Nickel, Ni 80.2 %
Phosphorus, P <= 0.0050 %
Silicon, Si 0.30 %
Sulfur, S <= 0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal
FloMet Permalloy® 4-79 Moly Soft Magnetic Alloy
Special Metals NILOMAG® Alloy 77
Goodfellow Nickel/Iron/Molybdenum Alloy
FloMet Fe-3% Si Soft Magnetic Alloy

NLEMO / 18004

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.