MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Kuraray SEPTON® PM4 Polypropylene Modified Plastic
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber; Polypropylene (PP)

Material Notes: Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic block copolymers, which exhibit rubber-like properties over a wide range of temperatures. SEPTON®'s characteristics include:
  • Excellent Mechanical Properties
  • Good Weatherability
  • Excellent Low Temperature Properties
  • Excellent Electrical Properties
  • Superior Heat Resistance
  • Excellent Chemical Resistance
  • Low Toxicity

SEPTON® grades are available with a range of Shore A hardness of 35-95 and tensile strengths of 290-5600 psi. SEPTON® resins are highly extendible with fillers, resins and oils, which allows formulation of a variety of hardness for adhesives, sealants and various compounds. As an additive, SEPTON® resins can be used to improve toughness of a variety of plastics. Several SEPTON® grades have U.S. FDA and USP Class VI approval.

SEPTON® has a versatile series of grades which can be used in numerous processing techniques such as blow molding, injection molding, extrusion, hot melt and solution coatings. SEPTON® resins are thermoplastics therefore, the scrap is recyclable without significant loss of properties.

Formulation (parts by weight): PP (Block Copolymer) - 70, SEPTON® 2002 - 30

Information provided by The Kuraray Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 36 g/10 min
@Load 2.16 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 0.540 GPa
Izod Impact, Notched 673 J/m
 680 J/m
@Temperature -20.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kuraray HYBRAR® HD3 Thermoplastic Rubber-HDPE Blend
Kuraray SEPTON® S4033 Thermoplastic Rubber
Kuraray SEPTON® PM1 Polypropylene Modified Plastic
Kuraray SEPTON® PM2 Polypropylene Modified Plastic
Kuraray SEPTON® CM1 Compatibilizer

PKUR027 / 49416

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.