MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beijing Ranger Chem PBT-201-G10 Flame Retarding FR PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled; Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishing grades (94V-0, V-2) exist, and electrical properties exhibited are the highest of any thermoplastic. Low water absorption is exhibited, and excellent electrical properties (CTI and GWIT) are retained over extended periods of usages, even with widely varied temperature and humidity conditions. The surface of molded products is smooth, and a low coefficient of friction is exhibited. As the amount of friction is low, PBT is suitable for use in application requiring friction and wear properties. The material is exceptionally reliable, with small in-use dimensional variation, and superior molding stability and dimensional precision. Long-term chemical resistance is exceptional, and at room temperature, there is almost no degradation in properties after. Both unreinforced and reinforced grades exhibit exceptional flowability, and excellent processability.

Application: VCD drive frames\ Connectors\ Trimmers\ Switch buttons for gas-fired instantaneous water heaters\ Relay blocks\ Driers\ Rectifiers\ Outer handles\ Height sensor cases\ Door mirror stays\ Drive component housings\ Energy saving lamp.

Information provided by Beijing Ranger Chemical Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/cc
@Temperature 23.0 °C
ASTM D792
Moisture Absorption at Equilibrium 0.080 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0060 - 0.013 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 95.0 MPaASTM D638
Flexural Strength 140 MPaASTM D790
Flexural Modulus 6500 MPaASTM D790
Izod Impact, Notched (ISO) 6.00 kJ/m²ASTM D256
Izod Impact, Unnotched (ISO) 40.0 kJ/m²ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.10e+16 ohm-cm
@Thickness 2.00 mm
ASTM D257
Dielectric Constant 3.0
@Frequency 50 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Dielectric Loss Index 0.020
@Frequency 50 Hz
Tangent; ASTM D150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 205 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 195 °CASTM D648
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 °C
Melt Temperature 225 - 245 °C
Mold Temperature 60.0 - 80.0 °C
Injection Pressure 40.0 - 100 MPa
Back Pressure 4.00 - 15.0 MPa
Screw Speed <= 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC
G-10 Fiberglass Epoxy Laminate Sheet
Kingfa JH720 G10 10% Glass Fiber Reinforced PC
DuPont Mobility and Materials Crastin® T841FR1 NC010 PBTC-GF10FR(17)
Chengdu Polyster KLX-G11 PC Film & Sheet

PRANG076 / 93081

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.