MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics PVC type I®
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes:

information provided by GEHR

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ASTM D2240
Tensile Strength, Yield 7800 psiASTM D638
Modulus of Elasticity 440 ksiASTM D638
Flexural Strength 11000 psiASTM D638
Izod Impact, Notched 2.20 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µin/in-°FASTM D696
Melting Point 385 °FASTM D3418
Maximum Service Temperature, Air 140 °FUL 746B
Deflection Temperature at 1.8 MPa (264 psi) 158 °FASTM D648
Minimum Service Temperature, Air 5.00 °FUL 746B
 
Compliance PropertiesOriginal ValueComments
FDA YesPhysiological indifference
 
Descriptive Properties
Bondabilityyes
Physiological indifferenceNSF, 14+61
UV Stabilizationon request

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GEHR Plastics PVC type II®
Aearo E-A-R Specialty Composites Isodamp® C-1000 Series TPE
Mitsubishi Chemical Advanced Materials Ertalyte™ PET Polyester-semi-crystalline thermoplastic, extruded
Arkema KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Eastman Eastar GN101 PETG Copolyester

PGEHR002f / 192462

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.