MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sibur KF-Z Carbamide Formaldehyde Resin
Categories: Polymer; Thermoplastic

Material Notes: In binding materials for production of wood laminate, base of glues for wood materials, for impregnation of paper during production of synthetic veneer sheet, production of varnish, production of rods and forms in the metallurgical industry. Mixing of resin with water at 10-21°C in ratio of 2:1.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 10 - 20
@Temperature 19.5 - 20.5 °C
(L), in viscometer VM-246 with 6 mm nozzle diameter
 15 - 35
@Temperature 19.5 - 20.5 °C
(F), in viscometer VM-246 with 6 mm nozzle diameter
 
Processing PropertiesOriginal ValueComments
Gel Time 0.670 - 1.083 minAt 100°C
 
Descriptive Properties
Concentration of Hydrogen Ions7.5-8.7 pH
Mass Fraction of Dry Residue65-69%
Mass Fraction of Free Formaldehyde<0.9%
Ultimate Strength<1.5 MPaIn cutting of glue layer of plywood after 24 hours in water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIB072 / 67635

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.