MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Novamid® 1010N2 1ES NAT PA6 FR(30)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Injection Molding, Flame Retardant (Halogen free)

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccdry; ISO 1183
Moisture Absorption 3.00 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cmSim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cmSim. To ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 40.0 MPacond; ISO 527-1/-2
 80.0 MPadry; ISO 527-1/-2
Elongation at Break 5.0 %dry; ISO 527-1/-2
 >= 50 %cond; ISO 527-1/-2
Elongation at Yield 4.8 %dry; ISO 527-1/-2
 22 %cond; ISO 527-1/-2
Tensile Modulus 1.50 GPacond; ISO 527-1/-2
 3.60 GPadry; ISO 527-1/-2
Flexural Strength 46.0 MPacond; ISO 178
 120 MPadry; ISO 178
Flexural Modulus 1400 MPacond; ISO 178
 3600 MPadry; ISO 178
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature 23.0 °C
dry; ISO 179/1eU
 NB
@Temperature 23.0 °C
cond; ISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²
@Temperature 23.0 °C
dry; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
cond; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmdry; IEC 60093
Surface Resistance 2.00e+14 ohmcond; IEC 60093
Dielectric Constant 4.0
@Frequency 100 Hz
dry; IEC 60250
 4.0
@Frequency 1e+6 Hz
dry; IEC 60250
Dielectric Strength 26.0 kV/mmdry; IEC 60243-1
Dissipation Factor 0.010
@Frequency 100 Hz
dry; IEC 60250
 0.020
@Frequency 1e+6 Hz
dry; IEC 60250
Comparative Tracking Index 550 Vdry; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°Cdry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°Cdry; ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 192 °Cdry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 170 °Cdry; ISO 75-1/-2
Flammability, UL94 V-0
@Thickness 0.800 mm
dry; IEC 60695-11-10
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
Dry; IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry)
Envalior Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
Envalior Akulon® K225-KS PA6 FR(30), Dry, Flame Retardant, Heat Stabilized
Envalior Akulon® K225-KV PA6 FR(30)
Envalior Akulon® K222-KMV5 /A PA6-MD25 FR(30)

PDSM9874 / 161495

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.