MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott Sapphire Optical Window
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Sapphire, as one of the hardest, most durable and scratch resistant materials, offers a broad transmission range from UV to mid infrared wavelengths (250 – 5000 nm). It is able to withstand extreme environmental conditions and temperature changes. SCHOTT offers sapphire windows in different supply forms, dimensions, and in customized processing stages.Material:
  • Extreme hardness & high mechanical strength (withstands extreme environmental conditions)
  • Excellent thermal conductivity/heat resistance
  • High transmittance (UV to IR)
  • Low dn/dT
  • High electrical resistance (10e14 Ohm-cm)
  • High dielectric constant (9.39 from 1.0 MHz to 8.5 GHz)
Applications:
  • Infrared applications (e. g. radiometry, guidance, gas analysis, medicine, safety and security)
  • High-pressure and shock-loading applications (e.g. chamber or heater windows in chemical process equipment)
  • Optical applications (e.g. optical components from UV to IR)
  • Scratchproof sapphire watch glasses
Advantages:
  • SCHOTT offers sapphire material in optical quality
  • Customized characteristics concerning dimensions and shapes (round, square, and more, diameters up to 300 mm)
  • Polished surface and customized coating for different applications
  • Best Practice in sapphire processing due to long term experiences from handling optical materials
  • Usage of most advanced equipment and state-of-the-art metrology for manufacturing and quality control

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.98 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 1525 - 2000
Hardness, Mohs 9.0
Tensile Strength at Break 40000 - 60000 psi
Modulus of Elasticity 345 GPa
Flexural Strength 70000 - 130000 psi
Flexural Modulus 5.20e+6 psi
Compressive Modulus 5.50e+6 psi
Bulk Modulus 35000 ksi
Poissons Ratio 0.29
Shear Modulus 21500 ksi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cm
@Temperature 1000 °C
 1.00e+11 ohm-cm
@Temperature 500 °C
 1.00e+16 ohm-cm
@Temperature 25.0 °C
Dielectric Constant 9.4E perpendicular to c-axis
 11.5E parallel to c-axis
Dielectric Strength 48.0 kV/mm
Dissipation Factor 0.00010
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.40 µm/m-°C
@Temperature 25.0 - 800 °C
Specific Heat Capacity 0.774 J/g-°C
Thermal Conductivity 27.21 W/m-K
Melting Point 2040 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Mateck Sapphire (Al2O3)
Quartz (SiO2)
Mateck Sapphire Aluminium oxide Substrate, Al2O3
Fused Quartz

CSGT9926 / 183179

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.