MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

3M Scotch-Weld™ 3748 Hot Melt Adhesive
Categories: Polymer; Adhesive

Material Notes: Good thermal shock resistance; Non-corrosive to copper for many electronic applications and Bonds polyolefines

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 5000 cP
@Temperature 191 °C
5000 cP
@Temperature 375 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 1.72 MPa250 psiOn Douglas Fir
Peel Strength 3.16 kN/m18.0 plion canvas
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-2V-2
Ring & Ball Softening Point 144 °C291 °FASTM E28-99

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 3750 Tan Hot Melt Adhesive
3M Scotch-Weld™ 3764 Hot Melt Adhesive
3M Scotch-Weld™ 3731 Hot Melt Adhesive
3M Scotch-Weld™ 3748 VO Hot Melt Adhesive
3M Scotch-Weld™ 3747 Hot Melt Adhesive

PMM34089 / 168836

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.