MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celcon® FG40U01 Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Celcon acetal copolymer grade FG40U01 is a specifically developed product for non - woven fiber production using melt blown processing technology.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %at 50% RH; ISO 62
Water Absorption at Saturation 0.65 %ISO 62
Linear Mold Shrinkage 0.022 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cmISO 294-4
Melt Flow 40 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 67.0 MPa50 mm/min; ISO 527-2/1A
Tensile Modulus 2.83 GPa1 mm/min; ISO 527-2/1A
Flexural Modulus 2.82 GPaISO 178
Izod Impact, Notched (ISO) 4.60 kJ/m²ISO 180/1A
Charpy Impact, Notched 0.420 J/cm²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 11357-1,2,3
Deflection Temperature at 1.8 MPa (264 psi) 101 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Zone 1 360 °F
Zone 2 380 °F
Zone 3 380 °F
Zone 4 380 °F
Die Temperature 380 °F
 
Descriptive Properties
Air Pressure8 psiProcessing Condition
Air Temperature400°FProcessing Condition
Die to Collector Distance7 in Processing Condition
Melt Pressure500 psiProcessing Condition

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hostaform® C 52021 POM, Unfilled
Kolon KOCETAL® K900 Standard Grade Acetal Resin
Asahi Kasei TENAC™ 7054 Homopolymer Acetal (POM), High Flowability high cycle
Celanese Celcon® CF802 POM, Specialty
Network Polymers Kepital® F10-02

PHCW33 / 45974

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.