MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
China Tungsten NT5 Titanium Carbonitride Alloy
Categories: Ceramic; Carbide

Material Notes: Titanium carbonitride base alloy , also called cermets, with of high hardness, good red hard-ness and wear resistance, medium toughness, high  corrosion resistance to acids and alkalis and hi-temperature oxidation resistance, and low density, used as tool materials for manufacturing cars, tractors and other engine industries; bet for cutting of carbon steel, low and medium alloy steels, and gray cast iron; of high cutting speeds, long tool life and high surface finish also used in seal rings and housings in manufacturing of chemical engineering equipment.

Information provided by China Tungsten

Key Words: ISO P20, M05, K10
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 92
Flexural Strength 1300 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-6Al-4V (Grade 5), Annealed
China Tungsten YG11 Tungsten Carbide
Aluminum 7075-T73; 7075-T735x
Titanium, Ti
Carpenter Micro-Melt® M-3 Class 2 Alloy (AISI M3)

NCHIN081 / 78923

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.