MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC Asahiklin AE3000 Fluorinated Solvent
Categories: Fluid; Solvent

Material Notes: Asahiklin AE3000 is a fluorinated solvent used for cleaning, drying, and as a carrier solvent. This Hydrofluoroether (HFE-347pc-f) is a nonflammable solvent that has excellent material compatibility, low surface tension. Low Global Warming Potential, and Zero ODP.

Applications:

  • Precision cleaning of metals, alloys, composites, and plastics
  • Carrier solvent for fluorinated oils and greases
  • Carrier solvent for silicone oils
  • Drying agent after cleaning with hydrocarbons or alcohols
  • Particle removal
  • Replacement of HCFC, Dupornt™ Vertrel® & 3M™ Novec™ solvents
Benefits:
  • Non-flammable
  • Non-corrosive
  • Low global warming potential (GWP)
  • Zero ozone depletion potential (ODP)
  • Low surface tension, low viscosity, high liquid density
  • Excellent thermal, chemical, and hydrolytic stability
  • Superior drying property
  • Excellent permeability
  • Recyclable
  • Recoverable by simple distillation
  • Can be used with ultrasonics
  • No surfactants necessary

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.47 g/cc
 1.45 g/cc
@Temperature 35.0 °C
 1.50 g/cc
@Temperature 15.0 °C
Viscosity 0.6468 cP
 0.5586 cP
@Temperature 35.0 °C
 0.7056 cP
@Temperature 15.0 °C
 1.2936 cP
@Temperature -20.0 °C
Vapor Pressure 0.310 atm
 0.968 atm
@Temperature 22.0 °C
 1.94 atm
@Temperature 40.0 °C
Surface Tension 16.4 dynes/cm
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 163 J/g
@Temperature 39.0 °C
Melting Point -94.0 °C
Boiling Point 56.0 °C
 
Descriptive Properties
Global Warming Potential540
Material CompatibilityABSat boiling point for 3 days, <0.1% Weight change, <0.1% Linear Swell
 EPDMat boiling point for 3 days, <0.1% Weight change, <0.1% Linear Swell
 Fluorelastomerat boiling point for 3 days, >86% Weight change, >24% Linear Swell
 Polymethyl methacrylateat boiling point for 3 days, affected, affected
 Polypropyleneat boiling point for 3 days, <2.5% Weight change, <1.0% Linear Swell
 Polystyreneat boiling point for 3 days, <0.1% Weight change, <0.1% Linear Swell
 PTFEat boiling point for 3 days, <2.5% Weight change, <0.1% Linear Swell
 Silicon Rubberat boiling point for 3 days, <12.5% Weight change, <2.5% Linear Swell

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Delo® 400 SAE 50

PAGCX071 / 191180

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.