MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Magnesium
Magnesium Elektron - Service & Innovation in Magnesium

(Viewing data as-entered. Click here to return)
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual Mg surface treatments may be applied. Uses include motorsports and aerospace.

Key Words: UNS M12310; AMS 4429
Vendors: Magnesium Elektron is the world leader in high strength magnesium alloys in rolled, extruded and cast forms. Phone (303) 589-3189 or visit www.magnesium-elektron.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.82 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 65 - 75
Tensile Strength >= 36.0 ksiMinimum design value
 26.0 ksi
@Temperature 260 °C
Typical
 35.0 ksi
@Temperature 191 °C
Typical
 38.0 ksi
@Temperature 121 °C
Typical
 39.2 ksi
@Temperature -35.0 °C
Typical
 40.6 ksi
@Temperature 22.2 °C
Tensile Strength, Yield 21.0 ksi
@Strain 0.2 %,
Temperature 260 °C
Typical
 >= 21.0 ksi
@Strain 0.2 %,
Temperature 22.2 °C
Minimum design value
 23.0 ksi
@Strain 0.2 %,
Temperature 191 °C
Typical
 24.0 ksi
@Strain 0.2 %,
Temperature 121 °C
Typical
 24.7 ksi
@Strain 0.2 %,
Temperature 22.2 °C
Typical
Elongation at Break >= 2.0 %Minimum design value
 5.0 %Typical
 7.0 %
@Temperature -35.0 °C
Typical
Creep Strength 12000 psi
@Temperature 204 °C,
Time 1.98e+6 sec
0.1% creep strain
 14000 psi
@Temperature 204 °C,
Time 360000 sec
0.1% creep strain
 17000 psi
@Temperature 204 °C,
Time 234000 sec
0.1% creep strain
Modulus of Elasticity 6400 ksi
Compressive Yield Strength 24.4 ksi
@Strain 0.2 %
Typical
Compressive Strength 53.2 ksiTypical
Poissons Ratio 0.27
Fatigue Strength 16700 - 17400 psi
@# of Cycles 5.00e+7
Push-Pull; R = 0.1
Fracture Toughness 13.6 ksi-in½KIC
Shear Modulus 2520 ksiCalculated
Shear Strength 25000 psi
Charpy Impact 1.3 ft-lb
@Temperature -35.0 °C
Notched
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000946 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.8 µin/in-°F
Specific Heat Capacity 0.240 BTU/lb-°F
Thermal Conductivity 804 BTU-in/hr-ft²-°F
Melting Point 1013 - 1184 °F
Solidus 1013 °F
Liquidus 1184 °F
Maximum Service Temperature, Air 400 °F
 
Processing PropertiesOriginal ValueComments
Solution Temperature 520 °C
@Time 28800 sec
Follow with hot quench and aging
Aging Temperature 200 °C
@Time 57600 sec
Follow with air cool
 
Component Elements PropertiesOriginal ValueComments
Gadolinium, Gd 1.0 - 1.7 %
Magnesium, Mg 94.7 - 96.2 %as balance; includes saturation of Zr
Neodymium, Nd 2.6 - 3.1 %
Zinc, Zn 0.20 - 0.50 %
 
Descriptive Properties
Corrosion Resistance10 - 30 mpyASTM B117 salt spray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Magnesium Alloy
Magnesium Elektron Elektron® AZ31B Magnesium Extrusion Alloy, UNS M11311
Magnesium, Mg; Annealed Sheet
Magnesium, Mg; Hard-Rolled Sheet
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia

NMAGEL898 / 147647

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.