MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Epoxy, Cycloaliphatic, Molded
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cycloaliphatic, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cycloaliphatic, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Master Bond is a leading manufacturer of high performance epoxy adhesives, sealants, coatings, potting/encapsulation compounds and impregnation resins. Our epoxies include one and two part formulations that can be cured at room temperature, with heat or exposure to UV light. Special formulations feature high electrical and/or thermal conductivity and wide service temperature ranges. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 20.0 - 10000 cPAverage value: 1160 cP Grade Count:13
 1700 - 7000 cP
@Temperature 50.0 - 50.0 °C
Average value: 4050 cP Grade Count:4
Molecular Weight 160 - 227 g/molAverage value: 190 g/mol Grade Count:4
 
Processing PropertiesOriginal ValueComments
Pot Life 21.0 - 150 minAverage value: 46.6 min Grade Count:14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Cast, Unreinforced
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Overview of materials for Epoxy Molding Compound
SGL Carbon Group SIGRAFIL C® C30 T045 EPY Continuous Tow Carbon Fiber with 45k filaments, Epoxy Sizing

O1704 / 77889

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.