MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Brandenburger KV 3 Thermal Insulation Board
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset

Material Notes: This material is popular in applications where thermal and mechanical stress occur together. This material is based on a matrix of high temperature resistant polymers and special glass silk fabrics. Typical applications are thermally and mechanically high-stressed heated presses and moulds. Also KV 3 is used to insulate drop forge dies, in the design of soldering masks and in many other applications.

Information provided by Brandenburger Isoliertechnik GmbH&Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/cc
Water Absorption 0.075 %24 hrs; DIN 53 495
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 530 MPaEN 63
 330 MPa
@Temperature 200 °C
EN 63
Flexural Modulus 20.0 GPaEN 63
 18.0 GPa
@Temperature 200 °C
EN 63
Compressive Strength 600 MPaEN ISO 604
 400 MPa
@Temperature 200 °C
EN ISO 604
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 20.0 °C
DIN 53752
Thermal Conductivity 0.250 W/m-KDIN 52 612
Maximum Service Temperature, Air 240 °CLong Term
 250 °CShort Term

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Brandenburger GL-P Thermal Insulation Board
Brandenburger S 4000 Thermal Insulation Board
Brandenburger BRA-GLA SI Thermal Insulation Board
Brandenburger GL-M Thermal Insulation Board
Brandenburger S 4000 HT Thermal Insulation Board

PBRAND03 / 27715

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.