MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxy Technology EPO-TEK® H20E Electrically Conductive, Silver Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: Product Description: EPO-TEK® H20E is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also used extensively for thermal management applications due to its high thermal conductivity. It has proven itself to be extremely reliable over many years of service and is still the conductive adhesive of choice for new applications. Also available in a single component frozen syringe.

Advantages & Application Notes:

  • Processing info: It can be applied by many dispensing, stamping and screen printing techniques.
    • Dispensing: compatible with pressure/time delivery, auger screws, fluid jetting and G27 needles, in a single-component fashion.
    • Screen Printing: best using >200 metal mesh, with polymer squeegee blade with 80D hardness.
    • Stamping: small dots 6 mil in diameter can be realized.
  • Misc / Other notes:
    • Many technical papers written over 30-40 year lifetime.
    • Over 1 trillion chips attached at a single company: no failures, Six Sigma and Certified Parts Supplier award winner.
    • Versatility in curing techniques including box oven, SMT style tunnel oven, heater gun, hot plate, IR, convection, or inductor coil.
    • Many custom modified products available, for the following improvements: viscosity and appearance, flexibility and thermal conductivity.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.03 g/cc2.03 g/ccPart A
 3.07 g/cc3.07 g/ccPart B
Particle Size <= 45 µm<= 45 µm
Viscosity 220 - 3200 cP
@Temperature 23.0 °C
220 - 3200 cP
@Temperature 73.4 °F
100 rpm
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) 2.0 ppm2.0 ppm
Ionic Impurities - K (Potassium) 3.0 ppm3.0 ppm
Ionic Impurities - Cl (Chloride) 73 ppm73 ppm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575
Tensile Modulus 5.576 GPa808.7 ksiStorage
Shear Strength 10.17 MPa1475 psiLap
 >= 11.7 MPa>= 1700 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.00040 ohm-cm<= 0.00040 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 31.0 µm/m-°C17.2 µin/in-°FBelow Tg
 158 µm/m-°C87.8 µin/in-°FAbove Tg
Thermal Conductivity 2.50 W/m-K17.4 BTU-in/hr-ft²-°FBased on standard method: Laser Flash
 29.0 W/m-K201 BTU-in/hr-ft²-°FBased on Thermal Resistance Data: R = L x K-1x A-1
Maximum Service Temperature, Air 200 °C392 °FContinuous
 300 °C572 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 80.0 °C>= 176 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature 425 °C797 °FDegradation Temperature
 
Processing PropertiesMetricEnglishComments
Cure Time  5.00 min
@Temperature 150 °C
0.0833 hour
@Temperature 302 °F
 15.0 min
@Temperature 120 °C
0.250 hour
@Temperature 248 °F
 45.0 min
@Temperature 175 °C
0.750 hour
@Temperature 347 °F
Pot Life 3600 min3600 min
Shelf Life  12.0 Month
@Temperature 23.0 °C
12.0 Month
@Temperature 73.4 °F
 12.0 Month
@Temperature -40.0 °C
12.0 Month
@Temperature -40.0 °F
 
Descriptive Properties
ColorSilverPart A
 SilverPart B
ConsistencySmooth thixotropic paste
Ionic Impurities NH498 ppm
Mix Ratio by Weight1:1
Number of ComponentsTwo
Thixotropic Index4.63
Weight Loss0.59%200°C
 1.09%250°C
 1.67%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H20E-175 Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® H20E-MP Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® H20S Electrically Conductive, Silver Epoxy for Die Stamping
Epoxy Technology EPO-TEK® E3001-HV Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® H20E-8 Electrically Conductive, Silver Epoxy

PPOXYT027 / 141066

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.