MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay GEROPON® DOS/PG Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Identification: SODIUM DIOCTYLSULPHOSUCCINATE IN GLYCOL WATER SOLUTION

CAS: 577 – 11 – 7; 57 – 55 – 6; 7732 – 18 – 5

Solubility: Dispersible in water and polar solvents. Soluble in most aromatic solvents.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Wetting agent, emulsifier, de-emulsifier. Used in specialty cleaners, dewatering agent for flotation concentrates, oil spill clean-up blends. High flash point compatibility agent for herbicide SE formulations.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/cc
pH 5.0 - 7.05% in water; RPG02
 
Thermal PropertiesOriginal ValueComments
Pour Point <= 0.000 °C
Flash Point >= 100 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceLimpid liquidRPG31
CompositionActive content0.65
 Dry substance64-66%, RPG25
Ionic ChargeAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay GEROPON® DOS Surfactant
Solvay GEROPON® CYA/75 Surfactant
Solvay GEROPON® SDS Surfactant
Solvay GEROPON® HW 15 N Surfactant
Solvay GEROPON® HW 25 Surfactant

WRHOD121 / 137352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.