Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone Rubber Substrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications. Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation. |