MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex APEX® 4130 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Notes: 75°C Jacket; RoHS Compliant

Features: Good UV Resistance; Sunlight Resistant (720 hours)

Uses: Flexible Cord Jacketing

Forms: Pellets

Agency Ratings: UL QMTT2 .E73402

Wire Types: SJTW; STW; ST; SVT; SRDT; SJT

Processing Method: Extrusion

Additional Information:

Temperature Rating: 80°C

Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 113°C: 86%

Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 113°C: 110%

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8315 seconds; ASTM D2240
Tensile Strength at Break 2600 psiASTM D638
Elongation at Break 360 %ASTM D638
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 167 °FContinuous Use; ASTM D794
Brittleness Temperature -16.6 °FASTM D746
Oxygen Index 29 %ASTM D2863
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex APEX® 84842 Polyvinyl Chloride, Flexible
Teknor Apex APEX® 80853-A Polyvinyl Chloride, Flexible
Teknor Apex APEX® 80851-F Polyvinyl Chloride, Flexible
Teknor Apex APEX® 80851-B Polyvinyl Chloride, Flexible
Teknor Apex APEX® 80851 Polyvinyl Chloride, Flexible

PTEKNO490 / 128667

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.