MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Bynel® 4157 Adhesive Resin
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.

Applications:Bynel® Series 4100 resins adhere to a variety of materials. They are most often used to adhere to EVOH, polyamide, PE, ionomers, and ethylene copolymers.

Bynel® Series 4100 resins can be used in coextrusion processes including:

  • blown film
  • cast film/sheet
  • blow molding melt and solid phase thermoforming
  • sheet and tubing
  • Bynel® 4157 can also be used in coextrusion coating. LLDPE resins are known for their temperature resistance, clarity and toughness. These physical properties make the Bynel® Series 4100 resins work well in applications such as:

  • boil-in-bag structures
  • blow molded containers in which drop strength is important
  • bag-in-box films
  • film where LLDPE is the heat seal layer

    Information provided by DuPont™

    This former DuPont product line is now a Dow product line.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.920 g/ccASTM D792
    Melt Flow 3.0 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    ASTM D1238
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 112 °CFreezing Point, DSC; ASTM D3418
     127 °CDSC; ASTM D3418
    Vicat Softening Point 93.0 °CASTM D1525
     
    Processing PropertiesOriginal ValueComments
    Rear Barrel Temperature 120 °CFor high temperature coextrusions.
     120 °CFor coextrusion with EVA or EVOH.
    Middle Barrel Temperature 220 °CFor coextrusion with EVA or EVOH.
     235 °CFor high temperature coextrusions.
    Front Barrel Temperature 235 °CFor coextrusion with EVA or EVOH.
     250 °CFor high temperature coextrusions.
    Adapter Temperature 235 °CFor coextrusion with EVA or EVOH.
     250 °CFor high temperature coextrusions.
    Die Temperature 455 °FFor coextrusion with EVA or EVOH.
     482 °FFor high temperature coextrusions.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Dow Bynel® 22E757 Modified Ethylene Acrylate
    Dow Bynel® 41E687 Adhesive Resin
    Dow Bynel® 4206 Anhydride-Modified LDPE Adhesive Resin
    Dow Bynel® 4105 Anhydride-Modified LLDPE Adhesive Resin
    Dow Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin

    PDUP908 / 33475

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.