MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ArcelorMittal 54 High formability steel for drawing, Cold rolled
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Available in the following: Extragal®/Galvannealed (DX54D +Z/+ZF)

Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the automotive industry, both for visible and structural parts. The guaranteed low scatter in their mechanical properties ensures optimum productivity in drawing press operations. The range of cold rolled steels has been extended to include the ultra high drawability quality. ArcelorMittal 07, ensuring maximum efficiency in the production of the most difficult- to-form parts (body sides, door liners, tailgates, etc.). The range of ArcelorMittal hot rolled mild steels covers the four levels of drawing difficulty listed below:

  • ArcelorMittal 12: for drawing, with minimum guaranteed yield strength
  • ArcelorMittal 13: for deep drawing
  • ArcelorMittal 14: for very deep drawing
  • ArcelorMittal 15: for drawing particularly difficult parts requiring performance regularity at high production rates (transfer presses).
These ArcelorMittal steel grades are non-ageing, conserving their mechanical properties and their formability over time. They are also suitable for class 1 hot dip galvanizing according to the EN 36503 standard. The ArcelorMittal range offers better guarantees than the usual standard-compliant drawing steels, while remaining compatible with standards.

Applications: These ArcelorMittal steels are designed for deep and extra deep drawing of visible and structural parts.

Information provided by ArcelorMittal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 280 - 340 MPa
Tensile Strength, Yield 160 - 200 MPa
Elongation at Break >= 38 %L0=80 mm, th<3 mm
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Iron, Fe >= 99.32 %as balance
Manganese, Mn <= 0.50 %
Silicon, Si <= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ArcelorMittal 51 High formability steel for drawing, Cold rolled
ArcelorMittal 52 High formability steel for drawing, Cold rolled
ArcelorMittal 53 High formability steel for drawing, Cold rolled
ArcelorMittal 56 High formability steel for drawing, Cold rolled
ArcelorMittal 57 High formability steel for drawing, Cold rolled

NARCE071 / 159979

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.