MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Niagara LaSalle CPO® Cold Finished Steel Bar
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Material Notes: CPO® chrome plated steel bars and tubes are manufactured to meet the specific needs for piston rod material in hydraulic and pneumatic cylinders. They are readily available in standard and custom sizes, chemistries and plating thicknesses to meet most piston rod applications.

Information provided by Niagra LaSalle Corporation

Key Words: AISI 1045; AISI 1050
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 69 - 71
Tensile Strength, Yield 50000 psi
@Thickness 15.9 - 152 mm
 >= 75000 psi
@Thickness 15.9 - 127 mm
 >= 100000 psi
@Thickness 15.9 - 114 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Niagara LaSalle IHCP® Cold Finished Steel Bar
AISI 1045 Steel, cold drawn, high temperature stress relieved, 50-75 mm (2-3 in) round
AISI 1045 Steel, Quenched and Tempered to 390 HB
JIS S45C Steel, Normalized
AISI 1045 Steel, cold drawn, annealed, 19-32 mm (0.75-1.25 in) round

NNIAL003 / 160293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.