MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® Shadowcure™ 5293 Silicone Coating
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes:
Conformal Coatings
Conformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Loctite offers both acrylic/urethane and silicone conformal coatings which are cured by UV, heat, or a two-part cure mechanism.

Loctite® 5293 Silicone  Shadowcure™ Coating
A silicone coating for severe temperature cycling environments and high reliability automotive use. Dual UV and moisture cure system. No solvents. Low VOC. Cure Type: UV or Moisture MIL-I-46058C Automotive; UL-746C Approved.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 600 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 70ASTM D2240
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 8.00e+16 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 secPrimary Cure is UV: Full Cure in 20-40 seconds @ 70 mW/cm^2. Secondary Cure is Moisture: Tack free in 2-6 hours, Full cure in 72 hours.
 
Descriptive Properties
ColorClear/Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 3-4170 DIELECTRIC GEL KIT
Aremco Heat-Away™ 641-EV Thermally Conductive Grease, Silver Filled, for High Vacuum Systems
Aremco AREMCOLOX™ 502-1400 (Full-Fired) Dense Alumina
Anderman Ceramics EC70P Mullite-Bonded Porous Silicon Carbide (70%)
A. Schulman Premi-Glas® 2550® AM CR-SX Fiberglass Reinforced Thermoset SMC

PLOCT176 / 51912

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.