MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unifrax Fiberfrax® Moist Pak-D® Ceramic Fiber Insulator
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax Moist Pak-D insulation is made from high-strength ceramic fiber blankets impregnated with inorganic bonding agents. This processing results in a flexible insulation that air dries to form a hard, rigid structure. Moist Pak-D is ideal for insulation of complex shapes and for service under conditions of high hot gas velocities.

The material is packaged in a clear polyethylene bag to retain the wet binder during shipment and storage. Since damage will occur, care should be taken to prevent freezing of the product.

Curing of product can be accomplished by air drying for several days or by immediate exposure to temperature in the application. Curing is merely a function of removing the water from the inorganic binder.

    Typical Applications
  • Hot face layer for Fiberfrax heater, furnace and kiln linings where hot gas velocities exceed 12.2 m/sec (40 ft/sec)
  • Hot gas duct, flue and stack linings
  • Recuperator linings
  • Blow pipe linings
  • External and internal pipe insulation
  • Reformer header insulation
  • Process furnace tube weld protection
  • Thermal and corrosion protection of process heater tube supports

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 12.0 - 18.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 17.0 psiWet; ASTM 686-76
 50.0 psiDry; ASTM 686-76
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.13 J/g-°C
@Temperature 1093 °C
Melting Point 1790 °C
Maximum Service Temperature, Air 1010 °CRecommended Operating Temperature
 
Component Elements PropertiesOriginal ValueComments
Al2O3 23 - 32 %
SiO2 68 - 77 %
 
Descriptive Properties
ColorWhite
Fiber Diameter (microns)2-3
Na2O3 (%)<0.5
Temperature Grade (°C)1093

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceraform 100 Ceramic Fiber
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator
Unifrax Fiberfrax® 110 Ceramic Fiber Paper
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator

CUNIF023 / 97795

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.