MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® A 8071 Acryl-divinylbenzene Copolymer Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® A 8017 is a strongly basic, gelular anion exchange resin (type I) based on an acryl-divinylbenzene copolymer of special bead size distribution. Due to its acrylic structure Lewatit A 8071 stands for effective adsorption and desorption of naturally occurring organic substances. Its very high total capacity and outstanding mechanical stability together with the excellent resistance to osmotic shock makes it unique of all demineralization applications especially if a low silica leakage is required. Lewatit A 8071 is especially suitable for:
  • demineralizing water later used for industrial steam generation operated with co-or counter-current systems such as Lewatit Liftbed System or Lewatit Rinsebed System
  • the removal of organic matter, especially from surface water
  • the extension of life time of acid baths in the finishing industry (acid retardation process)

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.730 g/cc
Density 1.09 g/cc
Bead Size 0.400 - 1.60 mm>90%
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceWhite, translucent
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polycasa Acryl® G 77 Acrylic, Injection Molding Grade
Polycasa Acryl® G 66 Acrylic, Injection Molding Grade
Polycasa Acryl® G 55 Acrylic, Injection Molding Grade
Polycasa Acryl® G 88 Acrylic
Polycasa Acryl® G 87 E Acrylic

PLANY8729 / 209122

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.