MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Mineral Filled

Material Notes: AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent dimensional stability and low moisture absorption. There are two versions of AMODEL A-1240 resin, "L" and "HS". The L version will usually provide the smoother, higher gloss surface, while the HS version gives better long-term thermal aging properties. Both AMODEL A-1240 resins can be easily processed using conventional equipment and methods.

This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.

MatWeb has an entry for this material conditioned at 50% RH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³ASTM D792
Water Absorption 0.14 %0.14 %24 hrs. ASTM D570
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM E831
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inASTM E831
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 125125ASTM D785
Tensile Strength, Ultimate 110 MPa16000 psiASTM D638
Elongation at Break 1.6 %1.6 %ASTM D638
Tensile Modulus 9.00 GPa1310 ksiASTM D638
Flexural Yield Strength 207 MPa30000 psiASTM D790
Flexural Modulus 7.60 GPa1100 ksiASTM D790
Poissons Ratio 0.290.29
Shear Modulus 3.49 GPa506 ksiCalculated
Shear Strength 96.0 MPa13900 psiASTM D732
Izod Impact, Notched 0.480 J/cm0.899 ft-lb/inASTM D256
Izod Impact, Unnotched 5.30 J/cm9.93 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 9.00e+15 ohm-cm9.00e+15 ohm-cmASTM D257
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
ASTM D150
 4.2
@Frequency 100 Hz
4.2
@Frequency 100 Hz
ASTM D150
Dissipation Factor  0.0060
@Frequency 100 Hz
0.0060
@Frequency 100 Hz
ASTM D150
 0.017
@Frequency 1e+6 Hz
0.017
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 125 sec125 secASTM D495
Comparative Tracking Index 550 V550 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear  34.0 µm/m-°C
@Temperature 0.000 - 100 °C
18.9 µin/in-°F
@Temperature 32.0 - 212 °F
FD; ASTM E831
 79.0 µm/m-°C
@Temperature 160 - 250 °C
43.9 µin/in-°F
@Temperature 320 - 482 °F
FD; ASTM E831
 95.0 µm/m-°C
@Temperature 160 - 250 °C
52.8 µin/in-°F
@Temperature 320 - 482 °F
TD; ASTM E831
CTE, linear, Transverse to Flow 40.0 µm/m-°C
@Temperature 0.000 - 100 °C
22.2 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM E381
Melting Point 310 °C590 °FASTM D3418
Maximum Service Temperature, Air 140 °C284 °F20,000 hours continuous use; ASTM D3045
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 154 °C309 °FASTM D648
Flammability, UL94  HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 321 - 343 °C610 - 649 °FInjection

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLVT40 / 21336

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.