MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAKEEP® 4000P PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP 4000P is an unreinforced, high viscosity polyether ether ketone powder. The product is suitable for the manufacture of compounds or it can be used as scatter powder for the manufacture of composites. The semi-crystalline polymer features superior thermal and chemical resistance. VESTAKEEP 4000P is self-extinguishing. VESTAKEEP 4000P is supplied as powder in boxes with moisture-proof polyethylene liners.

Information provided by Evonik

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Particle Size 550 µm550 µm
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 380 °C
11 g/10 min
@Load 11.0 lb,
Temperature 716 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 96.0 MPa13900 psiISO 527-1
Elongation at Break 30 %30 %ISO 527-1
Elongation at Yield 5.0 %5.0 %ISO 527-1
Tensile Modulus 3.50 GPa508 ksiISO 527-1
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 340 °C644 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75-1
Deflection Temperature at 1.8 MPa (264 psi) 150 °C302 °FISO 75-1
Vicat Softening Point  305 °C
@Load 5.10 kg
581 °F
@Load 11.2 lb
Method B; ISO 306
 335 °C
@Load 1.02 kg
635 °F
@Load 2.25 lb
Method A; ISO 306
Flammability, UL94 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
IEC60695

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Evonik VESTAKEEP® M4G PEEK
Ensinger Tecapeek® XP-96 Compression Molded PEEK
Evonik VESTAKEEP® 1000P PEEK
Evonik VESTAKEEP® 5000G PEEK

PEVONIL219 / 196423

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.