MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form as well as blended with other PE resins, such as LDPE or HDPE and mPE resins for mono extrusion of co-extrusion process to modify film properties.

Lotrene® Q2018 Series are suited for many applications in the field of consumer, industrial, food or hygiene packaging such as freezer film, bread bags, shoppers and bags as well as lamination film and multilayer packaging film.

Lotrene® Q2018C is a cast film grade and contains thermal stabilizers.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.918 g/ccISO 1183
Thickness 40.0 microns
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 0.000 ppm
Slip Level 0.000 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 11.0 MPaASTM D882
Film Tensile Strength at Yield, TD 11.0 MPaASTM D882
Film Elongation at Break, MD 850 %ASTM D882
Film Elongation at Break, TD 900 %ASTM D882
Elmendorf Tear Strength, MD 5.60 g/micronASTM D1922
Elmendorf Tear Strength, TD 10.7 g/micronASTM D1922
Dart Drop Test 130 gF50; ASTM D1709
Film Tensile Strength at Break, MD 35.0 MPaASTM D882
Film Tensile Strength at Break, TD 32.0 MPaASTM D882
1% Secant Modulus, MD 215 MPaASTM D882
1% Secant Modulus, TD 245 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 121 °CCrystalline; ISO 11357
Vicat Softening Point 100 °CASTM D1525 (A120)
 
Optical PropertiesOriginal ValueComments
Haze 14 %ASTM D1003
Gloss 55 %at 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 210 °CExtrusion
Melt Temperature 190 °C
Die Opening >= 0.180 cm
Blow-up Ratio (BUR) 2.0 - 3.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene
Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film
Chevron Phillips Marlex® 7120B LLDPE Blown & Cast Film Resin

PTOTAL767 / 130492

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.